Ø3.2x150mmthorium tungsten electrode price is USD1.326/PC on Jul. 27, 2017. WT20 is the most popular grade for
thorium tungsten electrode, and it has been the most expensive electrode
compared to other kinds, such as pure tungsten electrode, etc.
2017年7月28日星期五
2017年6月30日星期五
GTAW Safety
Welders wear protective clothing, including
light and thin leather gloves and protective long sleeve shirts with high
collars, to avoid exposure to strong ultraviolet light. Due to the absence of
smoke in GTAW, the electric arc light is not covered by fumes and particulate
matter as in stick welding or shielded metal arc welding, and thus is a great
deal brighter, subjecting operators to strong ultraviolet light. The welding
arc has a different range and strength of UV light wavelengths from sunlight,
but the welder is very close to the source and the light intensity is very
strong. Potential arc light damage includes accidental flashes to the eye or
arc eye and skin damage similar to strong sunburn. Operators wear opaque
helmets with dark eye lenses and full head and neck coverage to prevent this
exposure to UV light. Modern helmets often feature a liquid crystal-type face
plate that self-darkens upon exposure to the bright light of the struck arc.
Transparent welding curtains, made of a polyvinyl chloride plastic film, are
often used to shield nearby workers and bystanders from exposure to the UV light
from the electric arc.
Welders are also often exposed to dangerous
gases and particulate matter. While the process doesn't produce smoke, the
brightness of the arc in GTAW can break down surrounding air to form ozone and
nitric oxides. The ozone and nitric oxides react with lung tissue and moisture
to create nitric acid and ozone burn. Ozone and nitric oxide levels are
moderate, but exposure duration, repeated exposure, and the quality and
quantity of fume extraction, and air change in the room must be monitored.
Welders who do not work safely can contract emphysema and oedema of the lungs,
which can lead to early death. Similarly, the heat from the arc can cause
poisonous fumes to form from cleaning and degreasing materials. Cleaning
operations using these agents should not be performed near the site of welding,
and proper ventilation is necessary to protect the welder.
More details, please feel free to contact us by email sales@chinatungsten.com.
GTAW Technique
GTAW Welders often develop a technique of
rapidly alternating between moving the torch forward (to advance the weld pool)
and adding filler metal. The filler rod is withdrawn from the weld pool each
time the electrode advances, but it is always kept inside the gas shield to
prevent oxidation of its surface and contamination of the weld. Filler rods
composed of metals with a low melting temperature, such as aluminum, require
that the operator maintain some distance from the arc while staying inside the
gas shield. If held too close to the arc, the filler rod can melt before it
makes contact with the weld puddle. As the weld nears completion, the arc
current is often gradually reduced to allow the weld crater to solidify and
prevent the formation of crater cracks at the end of the weld.
More details, please feel free to contact us by email sales@chinatungsten.com.
GTAW Manual
Manual gas tungsten arc welding is a
relatively difficult welding method, due to the coordination required by the
welder. Similar to torch welding, GTAW normally requires two hands, since most
applications require that the welder manually feed a filler metal into the weld
area with one hand while manipulating the welding torch in the other.
Maintaining a short arc length, while preventing contact between the electrode
and the workpiece, is also important.
To strike the welding arc, a high frequency
generator (similar to a Tesla coil) provides an electric spark. This spark is a
conductive path for the welding current through the shielding gas and allows
the arc to be initiated while the electrode and the workpiece are separated,
typically about 1.5–3 mm (0.06–0.12 in) apart.
Once the arc is struck, the welder moves
the torch in a small circle to create a welding pool, the size of which depends
on the size of the electrode and the amount of current. While maintaining a
constant separation between the tungsten electrode and the workpiece, the operator then
moves the torch back slightly and tilts it backward about 10–15 degrees from
vertical. Filler metal is added manually to the front end of the weld pool as
it is needed.
More details, please feel free to contact us by email sales@chinatungsten.com.
History of GTAW - Plasma Arc Welding
Developments
continued during the following decades. Linde developed water-cooled torches
that helped prevent overheating when welding with high currents. During the
1950s, as the process continued to gain popularity, some users turned to carbon
dioxide as an alternative to the more expensive welding atmospheres consisting
of argon and helium, but this proved unacceptable for welding aluminum and
magnesium because it reduced weld quality, so it is rarely used with GTAW
today. The use of any shielding gas containing an oxygen compound, such as
carbon dioxide, quickly contaminates the tungsten electrode, making it
unsuitable for the TIG process. In 1953, a new process based on GTAW was
developed, called plasma arc welding. It affords greater control and improves
weld quality by using a nozzle to focus the electric arc, but is largely
limited to automated systems, whereas GTAW remains primarily a manual,
hand-held method. Development within the GTAW process has continued as well,
and today a number of variations exist. Among the most popular are the
pulsed-current, manual programmed, hot-wire, dabber, and increased penetration
GTAW methods.
More details, please feel free to contact us by email sales@chinatungsten.com.
History of GTAW - Heliarc
Russell
Meredith of Northrop Aircraft perfected the process in 1941. Meredith named the
process Heliarc because it used a tungsten electrode arc and helium as a
shielding gas, but it is often referred to as tungsten inert gas welding (TIG).
The American Welding Society's official term is gas tungsten arc welding
(GTAW). Linde Air Products developed a wide range of air-cooled and
water-cooled torches, gas lenses to improve shielding, and other accessories
that increased the use of the process. Initially, the electrode overheated
quickly and, despite tungsten's high melting temperature, particles of tungsten
were transferred to the weld. To address this problem, the polarity of the
electrode was changed from positive to negative, but the change made it
unsuitable for welding many non-ferrous materials. Finally, the development of
alternating current units made it possible to stabilize the arc and produce
high quality aluminum and magnesium welds.
More details, please feel free to contact us by email sales@chinatungsten.com.
History of GTAW - Gas-shielded Welding
The history of GTAW can be traced up to 19 century, which is by improving the welding and tungsten electrode is not the first material to be found for welding. After
the discovery of the short pulsed electric arc in 1800 by Humphry Davy and of
the continuous electric arc in 1802 by Vasily Petrov, arc welding developed
slowly. C. L. Coffin had the idea of welding in an inert gas atmosphere in
1890, but even in the early 20th century, welding non-ferrous materials such as
aluminum and magnesium remained difficult because these metals react rapidly
with the air and result in porous, dross-filled welds Processes using
flux-covered electrodes did not satisfactorily protect the weld area from
contamination. To solve the problem, bottled inert gases were used in the
beginning of the 1930s. A few years later, a direct current, gas-shielded
welding process emerged in the aircraft industry for welding magnesium.
More details, please feel free to contact us by email sales@chinatungsten.com.